CN 41-1243/TG ISSN 1006-852X
Volume 38 Issue 2
Apr.  2018
Turn off MathJax
Article Contents
SHAO Jingru, LI Fangyi, LIU Yongqi, LIU Zimu, ZHAI Xiangyang, ZHU Yibo, ZHANG Songfei, DONG Pei. Influence factors of electrolytic processing diamond blocks synthesizedby high temperature and high pressure catalyst method[J]. Diamond & Abrasives Engineering, 2018, 38(2): 12-14. doi: 10.13394/j.cnkij.gszz.2018.2.0003
Citation: SHAO Jingru, LI Fangyi, LIU Yongqi, LIU Zimu, ZHAI Xiangyang, ZHU Yibo, ZHANG Songfei, DONG Pei. Influence factors of electrolytic processing diamond blocks synthesizedby high temperature and high pressure catalyst method[J]. Diamond & Abrasives Engineering, 2018, 38(2): 12-14. doi: 10.13394/j.cnkij.gszz.2018.2.0003

Influence factors of electrolytic processing diamond blocks synthesizedby high temperature and high pressure catalyst method

doi: 10.13394/j.cnkij.gszz.2018.2.0003
More Information
  • Rev Recd Date: 2018-01-09
  • Available Online: 2022-07-07
  • Diamond is synthesized using graphite and metal catalyst at high temperature and high pressure. However, diamond in the synthetic block is tightly wrapped by graphite, catalyst metal and etc, which is difficult to purify through general physical methods. Electrolysis is used to oxidize the metal in the synthetic block on the anode into metal ions and thus solved in the solution, and then the ions are migrated to the cathode through the solution to recover the metal, which is a more efficient and environmentally friendly method at present. Through the electrolysis experiment, the influences of the main components of electrolyte and the conditions of electrolysis process on the efficiency of electrolysis are analyzed.The results show that the best mass concentration of activator in the additives is 15-30 g/L and the best mass concentration of composite stabilizer is 25-30 g/L, the additives can significantly improve the performance of electrolyte. The pH value of the electrolyte is 2-4, electric cathode and anode distance is 50-250 mm and the current of control cabinet is 4000-4200 A, the electrolysis efficiency can be significantly improved.

     

  • loading
  • 加载中

Catalog

    通讯作者: 陈斌, bchen63@163.com
    • 1. 

      沈阳化工大学材料科学与工程学院 沈阳 110142

    1. 本站搜索
    2. 百度学术搜索
    3. 万方数据库搜索
    4. CNKI搜索

    Article Metrics

    Article views (344) PDF downloads(12) Cited by()
    Proportional views
    Related

    /

    DownLoad:  Full-Size Img  PowerPoint
    Return