WANG Haikuo, ZHANG Xiangfa, WEI Xing, WANG Yongkai, REN Ying, ZHAO Haijun, LU Canhua, LIU Qiankun. Synthesizing bulk polycrystalline diamond by method of direct phase transition[J]. Diamond & Abrasives Engineering, 2018, 38(1): 1-6. doi: 10.13394/j.cnkij.gszz.2018.1.0001
Citation: WANG Haikuo, ZHANG Xiangfa, WEI Xing, WANG Yongkai, REN Ying, ZHAO Haijun, LU Canhua, LIU Qiankun. Synthesizing bulk polycrystalline diamond by method of direct phase transition[J]. Diamond & Abrasives Engineering, 2018, 38(1): 1-6. doi: 10.13394/j.cnkij.gszz.2018.1.0001

Synthesizing bulk polycrystalline diamond by method of direct phase transition

doi: 10.13394/j.cnkij.gszz.2018.1.0001
More Information
  • Rev Recd Date: 2017-12-28
  • Available Online: 2022-07-07
  • Pure-phase bulk polycrystalline diamonds are prepared through direct phase transition at ultrahigh pressure and high temperature. The phase composition and microstructure of the pure-phase bulk polycrystalline diamonds are studied by SEM, XRD and Raman spectrum. It is found that with different raw materials and different conditions, diamond samples have different colors and different grain sizes but they are all pure-phase polycrystalline diamonds.The average grain sizes for yellow-transparent and green samples are about 25 nm and 35 μm, respectively. The size of synthesized diamond blocks is φ6 mm×6 mm. The Vicker's hardness of yellow-transparent polycrystalline diamond, HV, is 130-270 GPa at the load of 3 N. According to China National Quality Supervision & Inspection Center for Abrasives, the abrasion ratio of yellow-transparent sample is 1.658×106, which is 25 times higher than that of commercial Co-based PCD used on oil bits. TG/DSC shows that the thermal stability of the yellow-transparent sample is almost the same as that of carat-level single-crystal diamond.Contrast grinding test, using NPD to grind against carat-level single-crystal diamond, shows that the abrasion ratio for the nano-structured polycrystalline diamond is 2.5, which demonstrates that the abrasion performance of NPD is much better than that of carat-level single-crystal diamond.

     

  • loading
  • 加载中

Catalog

    通讯作者: 陈斌, bchen63@163.com
    • 1. 

      沈阳化工大学材料科学与工程学院 沈阳 110142

    1. 本站搜索
    2. 百度学术搜索
    3. 万方数据库搜索
    4. CNKI搜索

    Article Metrics

    Article views (326) PDF downloads(12) Cited by()
    Proportional views
    Related

    /

    DownLoad:  Full-Size Img  PowerPoint
    Return
    Return